(via Thenewswire.ca)


Lomiko Metals Inc. (TSX-V: LMR; OTC: LMRMF; FSE: DH8B, Europe: ISIN:
CA54163Q1028, WKN: A0Q9W7) is pleased to announce that its 43-101
compliant report by Consul-Teck Exploration Services regarding the
Quatre Milles Flake Graphite Property located in southwestern Quebec
has been accepted by the TSX-Venture Exchange and has thus been filed
with Sedar (Canadian Securities Administrators).


Lomiko recently optioned the Quatre Milles Graphite Property in Quebec
to search for large flake, crystallite graphite which is sought after
for use in electric cars, fuel cells, pebble-bed nuclear reactors and
to create graphene, a newly discovered, chicken-wire shaped formation
of carbon which is one-atom thick and has incredible properties that
can make it 200 times stronger than steel, a superconductor at room
temperature and heat-resistant. Research scientists world-wide are
experimenting with new technology that uses graphene and at least 25
new patents have been filed.


Lomiko's Quatre Milles Graphite Property


The Quatre Milles Property is road accessible and is located
approximately 175 km northwest of Montreal and 17 km due north of the
village of Sainte-Veronique, Quebec. The property consists of 28
contiguous claims totaling approximately 1,600 hectares.


The property was originally staked and explored by Graphicor Resources
Inc. ("Graphicor") in the summer of 1989 based on the
results of a regional helicopter-borne EM survey. The underlying
geology consists of intercalated biotite gneiss, biotite feldspar
gneiss, marble, quartzite and calc-silicate lithologies of the Central
Metasedimentary Belt of the Grenville Province.


Historical Highlights


-Graphicor completed reconnaissance mapping and prospecting as well as
ground geophysics and a 26 hole diamond drill program totaling 1,625
metres.


-The work identified several conductive trends in the central portion
of the property and at least three, relatively flat lying graphitic
beds.


-Three surface samples were collected and analyzed returning results
of 14.16% Cgf, 18.06% Cgf and 20.35% Cgf.


-23 of the initial 26 drill holes intersected graphite concentrations
with graphite concentration in range of 4.69% in hole Q90-1 to a
highlight of 8.07% Cgf over 28.60 metres in hole Q90-7.


-The highest individual assay was reported in hole Q90-10 reporting
15.48% Cgf over 0.50 metres.


A table of results from the 43-101 indicates:



------------------------------------------
|HOLE NO.|FROM(M)|TO(M)|WIDTH (M)|GRADE |
| | | | |(% CGP)|
|----------------------------------------|
|Q90-1 |8.94 |10.46|1.52 |7.33 |
|----------------------------------------|
|Q90-2 |28.68 |30.13|1.45 |10.38 |
|----------------------------------------|
|Q90-3 |16.23 |17.84|1.61 |4.09 |
|----------------------------------------|
|Q90-4 |9.4 |14.1 |4.7 |3.95 |
|----------------------------------------|
|Q90-5 |2 |3.90 |1.90 |2.07 |
|----------------------------------------|
|Q90-5 |22.13 |23.25|1.12 |10.52 |
|----------------------------------------|
|Q90-6 |32.54 |41.19|8.65 |8.07 |
|----------------------------------------|
|Q90-6 |43.47 |44.05|0.98 |3.87 |
|----------------------------------------|
|Q90-7 |3.94 |32.54|28.60 |8.07 |
|----------------------------------------|
|Q90-8 |1.54 |2.16 |0.62 |14.89 |
|----------------------------------------|
|Q90-8 |5.23 |8.05 |2.82 |7.45 |
|----------------------------------------|
|Q90-9 |2.05 |3.10 |1.05 |8.47 |
|----------------------------------------|
|Q90-9 |5.76 |6.8 |1.04 |10.86 |
|----------------------------------------|
|Q90-10 |2.14 |5.54 |3.40 |8.02 |
|----------------------------------------|
|Q90-10 |7.03 |7.61 |0.58 |10.59 |
|----------------------------------------|
|Q90-10 |8.53 |9.03 |0.50 |15.48 |
|----------------------------------------|
|Q90-10 |9.27 |11.24|1.97 |12.37 |
|----------------------------------------|
|Q90-10 |14.16 |15.46|1.30 |4.26 |
|----------------------------------------|
|Q90-11 |26.82 |34.02|7.20 |4.63 |
|----------------------------------------|
|Q90-12 |0.94 |8.53 |7.59 |8.60 |
|----------------------------------------|
|Q90-12 |38.16 |43.61|5.45 |3.79 |
|----------------------------------------|
|Q90-13 |0.69 |10.28|9.59 |4.64 |
|----------------------------------------|
|Q90-13 |40.95 |43.14|2.19 |3.82 |
|----------------------------------------|
|Q90-14 |5.56 |7.22 |1.66 |8.12 |
|----------------------------------------|
|Q90-15 |2.21 |5.59 |3.38 |9.76 |
|----------------------------------------|
|Q90-16 |? |? |? |NSV |
|----------------------------------------|
|Q90-17 |15.48 |18.63|3.15 |8.11 |
|----------------------------------------|
|Q90-17 |21.43 |23.67|2.24 |13.29 |
|----------------------------------------|
|Q90-17 |36.77 |47.97|11.20 |5.88 |
|----------------------------------------|
|Q90-17 |57.15 |58.21|1.06 |9.53 |
|----------------------------------------|
|Q90-17 |59.54 |69.82|10.28 |5.99 |
|----------------------------------------|
|Q90-18 |10.68 |12.90|2.22 |8.12 |
|----------------------------------------|
|Q90-19 |47.80 |49.25|1.45 |9.16 |
|----------------------------------------|
|Q90-19 |50.42 |58.49|8.07 |5.72 |
|----------------------------------------|
|Q90-20 |13.51 |16.98|3.47 |5.81 |
|----------------------------------------|
|Q90-21 |2.80 |4.98 |2.18 |5.56 |
|----------------------------------------|
|Q90-22 |17.37 |20.04|2.67 |2.58 |
|----------------------------------------|
|Q90-23 |? |? |? |NSV |
|----------------------------------------|
|Q90-24 |1.78 |4.14 |2.36 |3.77 |
|----------------------------------------|
|Q90-24 |12.32 |13.09|0.77 |4.20 |
|----------------------------------------|
|Q90-24 |16.86 |18.66|1.80 |4.96 |
|----------------------------------------|
|Q90-25 |19.69 |21.24|1.55 |3.67 |
|----------------------------------------|
|Q90-25 |25.27 |26.65|1.38 |9.66 |
|----------------------------------------|
|Q90-26 |? |? |? |NSV |
------------------------------------------


The Company cautions that it has not had the chance to verify the
quality and accuracy of the historic sampling and drilling results
reported in this news release which predate the introduction of NI
43-101 and cautions readers not to rely upon them. The historic
figures were generated from sources believed to be reliable, however,
they have not been confirmed. Although the sampling and drilling
results are relevant, they have not been verified.


Graphite Market


-The price for flake graphite is $ 2000-$3000 per tonne depending on
flake size and grade.


-Graphite prices have been increasing in recent months and over the
last couple of years prices for large flake, high purity graphite (+80
mesh, 94-97%C) have more than doubled.


-Graphite prices have almost tripled since 2005 due to the ongoing
industrialization of China, India and other emerging economies and
resultant strong demand from traditional steel and automotive markets.


-Demand for graphite is expected to rise as electric vehicles and
lithium battery technology are adopted, nuclear reactors are built in
China, and if fuel cells and graphene patents become products.


-China, which produces about 70 per cent of the world's graphite, is
seeing production and export growth leveling, and export taxes and a
licensing system have been instituted.


-Europe and the USA have both indicated graphite is of economic
importance and has a supply risk (Critical Raw Materials for the EU,
July 2010).


Graphite Facts


-Natural graphite comes in several forms: flake, amorphous and lump.


-Southwestern Quebec is host to some of the most favorable geological
terrain for graphite exploration in Canada and is known to host
graphite resources, including the nearby Lac Des Iles mine operated by
Timcal.


-Graphite has many important new applications such as lithium-ion
batteries, fuel cells, and nuclear and solar power that have the
potential to create significant incremental demand growth.


-There is roughly 20-30 times more graphite by weight needed to
produce a lithium-ion battery than there is lithium.


-Of the 1.2 million tonnes of graphite produced annually,
approximately 40 per cent is of the most desirable flake type.


-High-growth, high-value graphite applications require large-flake and
high-purity graphite which is the prime exploration and development
target at the Quatre Milles Property.


Near-Term Strategy


Lomiko plans to mount an aggressive exploration campaign on the Quatre
Milles Graphite Property commencing with a complete compilation of
historic geologic work followed by surface mapping, prospecting and
follow-up diamond drilling.


Jean-Sebastien Lavallee (OGQ #773), geologist, a Qualified Person as
defined by National Instrument 43-101, has reviewed and approved the
technical content of this release.


For more information, review the website at www.lomiko.com, or contact
A. Paul Gill at 604-729-5312 or by email at: info@lomiko.com.


On Behalf of the Board


"A. Paul Gill"


Chief Executive Officer


We seek safe harbor. Neither TSX Venture Exchange nor its Regulation
Services Provider (as that term is defined in the policies of the TSX
Venture Exchange) accepts responsibility for the adequacy or accuracy
of this release.

Copyright (c) 2012 Thenewswire.ca - All rights reserved.


Bewerten 
A A A
PDF Versenden Drucken

Für den Inhalt des Beitrages ist allein der Autor verantwortlich bzw. die aufgeführte Quelle. Bild- oder Filmrechte liegen beim Autor/Quelle bzw. bei der vom ihm benannten Quelle. Bei Übersetzungen können Fehler nicht ausgeschlossen werden. Der vertretene Standpunkt eines Autors spiegelt generell nicht die Meinung des Webseiten-Betreibers wieder. Mittels der Veröffentlichung will dieser lediglich ein pluralistisches Meinungsbild darstellen. Direkte oder indirekte Aussagen in einem Beitrag stellen keinerlei Aufforderung zum Kauf-/Verkauf von Wertpapieren dar. Wir wehren uns gegen jede Form von Hass, Diskriminierung und Verletzung der Menschenwürde. Beachten Sie bitte auch unsere AGB/Disclaimer!




Mineninfo
Lomiko Metals Inc.
Bergbau
A40GBL
CA54163Q8056
Minenprofile
Alle Angaben ohne Gewähr! Copyright © by GoldSeiten.de 1999-2024.
Die Reproduktion, Modifikation oder Verwendung der Inhalte ganz oder teilweise ohne schriftliche Genehmigung ist untersagt!

"Wir weisen Sie ausdrücklich auf unser virtuelles Hausrecht hin!"